AMS 5661/USN N09901 Taflen Superalloy ar gyfer Tyrbin Nwy Incoloy 901 Plât Alloy Nickel
Fel cyflenwr a gwneuthurwr blaenllaw yn Tsieina, mae GNEE Steel yn darparu cynhyrchion aloi cost-effeithiol sy'n seiliedig ar nicel.
- Anfon e-bost:ss@gneesteel.com
- Ffôn:+8615824687445
Alloy 901 is an age-hardenable super alloy which contains Titanium and Aluminium for precipitation hardening and molybdenum for soild-solution strengthening. Alloy 901 has high yield strength and creep resistance at temperatures to about 1110℃F (600℃). As Alloy 901 has a substantial iron content it enables alloy 901 to combine strength with good Defnyddir nodweddion ffugio . aloi 901 yn gyffredin ar gyfer disgiau injan tyrbin nwy, siafftiau, modrwyau, casinau a morloi .
Cais Incoloy 901
Tyrbin nwy
▪ Peiriant awyrennau
Modrwy allanol tyrbin
▪ Clymwr
Manylebau incoloy 901
▪ UNS N09901
▪ Rhif Werkstoff 2.4662
▪ Br hr 55
▪ AMS 5660
▪ AMS 5661
▪ Aecma pren2176
▪ Aecma pren2177
▪ ISO 9723
▪ ISO 9725
▪ MSRR 7029, MSRR 7031
▪ Alloy Nimonig 901
Incoloy 901Gyfansoddiad cemegol
| Elfen | Cynnwys (%) |
| Nicel, ni | 40-45 |
| Haearn, fe | 33 |
| Cromiwm, cr | 11-14 |
| Molybdenwm, MO | 5.0 - 6.50 |
| Titaniwm, ti | 2.80-3.10 |
| Cobalt, CO | 1 |
| Manganîs, MN | 0.50 |
| Copr, cu | 0.50 |
| Silicon, si | 0.40 |
| Alwminiwm, al | 0.35 |
| Carbon, c | 0.10 |
| Sylffwr, s | 0.030 |
Ein cwmni


Tagiau poblogaidd: AMS 5661/USN N09901 Taflen Superalloy ar gyfer Tyrbin Nwy Incoloy 901 Plât Alloy Nickel, China AMS 5661/USN N09901 Taflen Superalloy ar gyfer Tyrbin Nwy Incoloy 901 Cyflenwyr Alloy Nickel Nickel
Fe allech Chi Hoffi Hefyd
Anfon ymchwiliad













